Feritová jádra RM


|
Modelka |
G.W |
VELIKOST (mm) |
||||||||
|
A1 |
A |
B |
C |
D |
E |
F |
Gmin |
H |
||
|
RM6 |
5.6 |
14.4±0.3 |
17.55±0.35 |
12.65±0.25 |
8.0±0.2 |
6.3±0.1 |
4.1±0.1 |
8.8±0.1 |
8.8 |
10.3±0.3 |
|
RM8 |
13.6 |
19.3±0.4 |
22.7±0.5 |
17.3±0.3 |
10.7±0.3 |
8.4±0.2 |
5.5±0.1 |
11.4±0.5 |
9.5 |
14.3±0.3 |
|
RM10 |
24 |
24.1±0.6 |
27.8±0.7 |
21.6±0.5 |
13.2±0.3 |
10.7±0.2 |
6.3±0.2 |
9.3±0.1 |
10.9 |
16.2±0.3 |
|
RM12 |
49 |
29.2±0.6 |
36.7±0.7 |
25.5±0.5 |
15.8±0.3 |
12.6±0.2 |
8.5±0.2 |
11.85±0.1 |
16.8 |
21.6±0.3 |
|
RM14 řekl: |
77 |
34.1±0.6 |
41.5±0.7 |
29.6±0.6 |
18.7±0.3 |
14.7±0.3 |
10.6±0.1 |
15.5±0.1 |
17.0 |
27.0±0.3 |
|
MODELKA |
PARAMETR |
AL±25 %(nH/N^2) |
N.W(g) |
|||||||
|
C1 mm-1 |
Lemm |
Aemm2 |
Vemm3 |
ZP40 |
ZH7K |
ZH10K |
||||
|
RM6 |
0.784 |
29.2 |
37.0 |
1090.0 |
2150 |
6000 |
8600 |
4.9 |
||
|
RM8 |
0.604 |
38.4 |
63.0 |
2440.0 |
3300 |
8750 |
12500 |
12.0 |
||
|
RM10 |
0.462 |
44.6 |
96.6 |
43100.0 |
4000 |
11200 |
16000 |
22.0 |
||
|
RM12 |
0.388 |
56.6 |
146.0 |
8340.0 |
5000 |
13000 |
17700 |
45.0 |
||
|
RM14 řekl: |
0.35 |
70 |
198.0 |
13900.0 |
5700 |
14500 |
19600 |
67.0 |
||
Populární Tagy: feritová rm jádra, Čína výrobci feritových rm jader, dodavatelé, továrna