FERITOVÁ L JÁDRA

FERITOVÁ L JÁDRA

product-433-375

 

MODELKA

G.W

VELIKOST

N.W

A

B

C

L59.5/32/36

338

59.5±1.0

32.0±0.5

36.0±0.5

329

L60.9/32/38

362

60.9±1.0

32.0±0.5

38.0±0.5

355

L60/16/8

41

60.0±1.5

16.0±0.5

8.0±0.3

38

L70/66/17

407

70.0±1.0

66.0±0.6

17.0±0.3

380

L71/42.5/16.5

260

71.0±0.5

42.5±0.6

16.5±0.3

239

L73/35/16

207

73.0±1.5

35.0±1.0

16.2±0.2

193

L78/66/28

750

78.0±1.0

66.0±0.8

28.0±0.4

680

L96/32/38

580

96.0±1.5

32.0±0.5

38.0±0.5

560

L101.6/50.8/25.4

660

101.6±1.0

50.8±0.5

25.4±0.65

625

L114.3/50.8/25.4

744

114.3±1.0

50.8±0.5

25.4±0.65

700

Populární Tagy: feritová l jádra, Čína výrobci feritových l jader, dodavatelé, továrna

Odeslat dotaz