For soft magnetic alloys, even in weak magnetic fields, a narrow hysteresis loop can be induced, which makes this type of alloy potentially applicable in some new fields, such as high-frequency induction. Currently, scholars have conducted extensive research in this field, utilizing soft magnetic materials to pair microelectronic sensors to improve their performance, reduce the size of sensor components, and fully utilize the high magnetic permeability characteristics of soft magnetic materials.
A basic feature of magnetic materials is that they are placed in a magnetic field to interact with their internal magnetic moments, resulting in a direction consistent with the applied external magnetic field, which is commonly known as "magnetization". Magnetization is divided into spontaneous magnetization and non spontaneous magnetization. If the internal magnetic moments of the material are completely reversed, the magnetization of the material is {{0}}; if the magnetic moments are arranged regularly in a certain direction, the magnetization of the material is not 0.
When a magnetic material is subjected to an external magnetic field, its magnetic moment direction will rotate in the direction of the external magnetic field. This means that the material exhibits anisotropy and enhances in the direction of the applied external magnetic field. The high-frequency performance of such materials can be characterized by their intrinsic properties under a certain magnetic field.
On the one hand, this environmental sensitivity can be used to modify magnetic materials. If the original material has good performance at low frequencies, apply a suitable magnetic field in a certain direction to improve its high-frequency characteristics. On the other hand, due to the presence of magnetic inclusions, the performance of mobile phone filters can be affected by the geomagnetic field, and this effect is harmful.